Data on the evolution of curing characteristics and properties during the room-temperature annealing process in SSBR/BR gums and SSBR/BR/SiO2 composites

机译:SSBR / BR胶和SSBR / BR / SiO2复合材料在室温退火过程中固化特性和性能演变的数据

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

The present article contains the data of tensile stress-strain curves, crosslinking characteristics curves, filler dispersion images and dynamic mechanical properties of SSBR/BR blends and SSBR/BR/SiO composites during room-temperature annealing. The data in this article aims to accurately describe the evolution of the network structures and physical mechanical properties of rubber composites during annealing process. Tensile stress-strain curves of un-vulcanized rubber gums and compounds were obtained by an electrical tensile tester with a speed of 100 mm/min. The crosslinking characteristics of the un-vulcanized rubber blends or composites after different annealing time were measured by a rotor-free vulcameter at 150 °C. The macroscopic filler dispersion of the filled vulcanizates was analyzed on a smooth cross-section of cut rubber. The dynamic mechanical properties of vulcanized SSBR/BR blends and SSBR/BR/SiO composites were investigated by a dynamic mechanical thermal analyser with different temperature ranges and strains. These findings may serve as references for the scientific processing of green tire materials in automotive industry, and this article is related to our research article entitled “Effect of room-temperature annealing on structures and properties of SSBR/BR blends and SSBR/BR/SiO composites” (Xinping Zhang et al., 2019).
机译:本文包含了室温退火过程中SSBR / BR共混物和SSBR / BR / SiO复合物的拉伸应力-应变曲线,交联特性曲线,填料分散图像和动态力学性能的数据。本文中的数据旨在准确描述退火过程中橡胶复合材料的网络结构和物理力学性能的演变。未硫化的橡胶胶和胶料的拉伸应力-应变曲线通过电拉伸试验机以100mm / min的速度获得。未硫化的橡胶混合物或复合物在不同的退火时间后的交联特性是通过无转子的硫化计在150°C下测量的。在切胶的光滑横截面上分析了填充的硫化橡胶的宏观填料分散体。通过动态机械热分析仪研究了不同温度范围和应变的硫化SSBR / BR共混物和SSBR / BR / SiO复合材料的动态力学性能。这些发现可为汽车工业中生胎材料的科学加工提供参考,并且与我们的研究文章“室温退火对SSBR / BR共混物和SSBR / BR / SiO的结构和性能的影响有关。复合材料''(Xinping Zhang et al。,2019)。