A Comparitive Evaluation of the Marginal Adaptation of Zirconium Coping and Nickel–Chromium Coping Using Shoulder Finish Line Design: An Invitro Study

机译:肩部终点线设计对锆合金和镍铬合金的边际适应性的比较评估:一项体外研究

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

Marginal adaptation is an important factor for long term clinical success of the restoration. This study aims to evaluate and compare the marginal adaptation of zirconium coping and nickel–chromium coping using the shoulder finish line design. For the purpose of this study 30 master dies were fabricated. A total of 30 copings were fabricated in which 15 zirconia copings and 15 Ni–Cr copings were fabricated. The copings obtained were seated on the die and marginal discrepancy between the metal die and the copings were then measured with Scanning electron microscope at magnification of ×50 and the findings were statistically analyzed. Mean and standard deviation values of marginal discrepancy of cervical margins of zirconia copings were 39.32 and 2.66 μm and Ni–Cr copings were 129.98 and 2.57 μm. Higher mean marginal gap (μm) is recorded in Ni–Cr copings compared to zirconia copings. The difference in mean marginal gap (μm) between the two copings is found to be statistically significant (P < 0.001). Within the limitation of this study it was concluded that higher mean marginal gap (μm) was recorded in Ni–Cr copings compared to zirconia copings. The difference in mean marginal gap (μm) between the two copings is found to be statistically significant (P < 0.001).
机译:边缘适应是修复长期临床成功的重要因素。本研究旨在评估和比较采用肩部终点线设计的锆合金顶盖和镍铬合金顶盖的边际适应性。为了该研究的目的,制造了30个母模。总共制作了30个顶盖,其中制作了15个氧化锆顶盖和15个Ni-Cr顶盖。将获得的顶盖放置在模具上,然后用扫描电子显微镜以×50的放大倍数测量金属模具和顶盖之间的边际差异,并对结果进行统计分析。氧化锆顶盖的宫颈边缘的边缘差异的平均值和标准偏差值为39.32和2.66μm,而Ni-Cr顶盖的颈部差异为129.98和2.57μm。与氧化锆顶盖相比,Ni-Cr顶盖的平均边际间隙(μm)更高。发现两次应对之间的平均边缘间隙(μm)的差异具有统计学显着性(P <0.001)。在本研究的范围内,得出的结论是,与氧化锆顶盖相比,Ni-Cr顶盖的平均边际间隙(μm)更高。发现两次应对之间的平均边缘间隙(μm)的差异具有统计学显着性(P <0.001)。