This paper examines the influence of a short-term thermal treatment of aerosol deposited negative temperature coefficient (NTC) thermistor films on the NTCR characteristics and their long-term stability with different electrode materials. An aerosol deposition of a spinel-based NiMn2O4 powder on alumina substrates with screen-printed AgPd and Au interdigital electrode structures was performed. The manufactured components of the typical size of 1206 were tempered in a moderate temperature range of 200 °C to 800 °C and aged for 1000 h at 125 °C in air. Based on R-T measurements in a high-precision silicone oil thermostat bath and high temperature XRD analyses, the influence of the thermal treatment was analyzed and discussed. A 60-min tempering at 400 °C proved to be optimal, as both the NTCR parameters and their ageing stability could be significantly improved. The findings are explained.
机译:本文研究了短期热处理气溶胶沉积负温度系数(NTC)热敏电阻膜对NTCR特性及其在不同电极材料下的长期稳定性的影响。在具有丝网印刷的AgPd和Au叉指电极结构的氧化铝基板上进行了尖晶石型NiMn2O4粉末的气溶胶沉积。将制造的典型尺寸为1206的组件在200°C至800°C的中等温度范围内进行回火,并在125°C的空气中老化1000 h。基于高精度硅油恒温槽中的R-T测量和高温XRD分析,分析和讨论了热处理的影响。事实证明,在400°C下进行60分钟的回火是最佳的,因为NTCR参数及其老化稳定性都可以得到显着改善。研究结果进行了解释。