Purity, morphology, and structural characterization of synthesized deep eutectic solvent (DES)-lignins (D6h, D9h, D12h, D18h, D24h) extracted from willow (Salix matsudana cv. Zhuliu) after treatment with a 1:10 molar ratio of choline chloride and lactic acid at 120 °C for 6, 9, 12, 18, and 24 h were carried out. The purity of DES-lignin was ~95.4%. The proportion of hydrogen (H) in DES-lignin samples increased from 4.22% to 6.90% with lignin extraction time. The DES-lignin samples had low number/weight average molecular weights (1348.1/1806.7 to 920.2/1042.5 g/mol, from D6h to D24h) and low particle sizes (702–400 nm). Atomic force microscopy (AFM) analysis demonstrated that DES-lignin nanoparticles had smooth surfaces and diameters of 200–420 nm. Syringyl (S) units were dominant, and total phenolic hydroxyl content and total hydroxyl content reached their highest values of 2.05 and 3.42 mmol·g−1 in D12h and D6h, respectively. β-Aryl ether (β-O-4) linkages were eliminated during DES treatment.
机译:从柳树(Salix matsudana cv。Zhuliu)中提取的合成深共熔溶剂(DES)-木质素(D6h,D9h,D12h,D18h,D24h)的纯度,形态和结构表征,以1:10摩尔比的氯化胆碱处理乳酸在120℃下进行6、9、12、18和24小时。 DES-木质素的纯度约为95.4%。随着木质素提取时间的增加,DES-木质素样品中的氢(H)比例从4.22%增加到6.90%。 DES-木质素样品的数均/重均分子量低(从D6h到D24h从1348.1 / 1806.7到920.2 / 1042.5 g / mol)和低粒径(702-400 nm)。原子力显微镜(AFM)分析表明,DES-木质素纳米颗粒具有光滑的表面,直径为200-420 nm。丁香基(S)单元占主导地位,在D12h和D6h中总酚羟基含量和总羟基含量分别达到2.05和3.42 mmol·g -1 的最高值。 DES处理期间消除了β-芳醚(β-O-4)的连接。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
代理获取

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号