>Objective: Oral rehabilitation success is enhanced by an accurate and reproducible final impression. The purpose of this study is to evaluate the dimensional changes of a polyether and addition silicone subjected to disinfection and/or sterilization after a long storage period. >Material and methods: Ninety samples were obtained from polyether ImpregumTM PentaTM (3M ESPETM, Seefeld, Germany) and 90 of addition silicone ImprintTM 4 PentaTM Putty (3M ESPETM, Seefeld, Germany) according to ISO 4823:2000. The samples of each material were split to form three groups with 30 samples each: a control group, a hypochlorite group (disinfection) and an autoclave group (sterilization). Samples were stored in the Portuguese Institute for Quality for six months at 23 °C. Samples were measured by laser interferometry, according to the Michelson technique before calculating dimensional stability according ISO 4823:2000. A statistical analysis via a three-way mixed ANOVA was performed. >Results: Significant shrinkage of ImpregumTM PentaTM was 0.77 ± 0.17% in the control group, 0.42 ± 0.19% in the hypochlorite group and 0.52 ± 0.28% in the autoclave group. For ImprintTM 4 PentaTM Putty, the control group had a shrinkage of 0.42 ± 0.12%, the hypochlorite group 0.36 ± 0.09% and the autoclave group 0.59 ± 0.13%. >Conclusions: The long-term storage of samples subjected to disinfection with 5.25% hypochlorite or autoclave sterilization can be used in a clinical setting as the dimensional changes are below the maximum permitted by the ISO 4823:2000, since there are no clinically significant changes in the dimension of the samples during the storage period.
机译:>目标:准确和可复制的最终印象可提高口腔康复的成功率。这项研究的目的是评估经过长时间保存后经过消毒和/或灭菌的聚醚和加成硅酮的尺寸变化。 >材料和方法:90份样品是从德国Seefeld的聚醚Impregum TM Penta TM (3M ESPE TM )获得的)和90的附加有机硅Imprint TM 4 Penta TM 腻子(3M ESPE TM ,德国塞费尔德),根据ISO 4823:2000。将每种材料的样品分成三组,每组30个样品:对照组,次氯酸盐组(消毒)和高压灭菌组(灭菌)。样品在23°C下在葡萄牙质量研究所保存了六个月。在根据ISO 4823:2000计算尺寸稳定性之前,根据迈克尔逊技术,通过激光干涉术测量样品。通过三向混合方差分析进行统计分析。 >结果:Impregum TM Penta TM 的收缩率在对照组为0.77±0.17%,在次氯酸盐组为0.42±0.19%,在0.52为0.52高压灭菌器组为±0.28%。对于Imprint TM 4 Penta TM 腻子,对照组收缩率为0.42±±0.12%,次氯酸盐组收缩率为0.36±±0.09%,高压灭菌器组收缩率为0.59±0.13%。 >结论:由于尺寸变化低于ISO 4823:2000所允许的最大值,因此可在临床环境中长期使用5.25%次氯酸盐或高压灭菌器消毒的样品。在储存期间,样品的尺寸没有临床上的显着变化。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
代理获取

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号