PURPOSE Vinyl polyether silicone (VPES) has a different composition from other elastomeric impression materials as it combines vinyl polysiloxane (VPS) and polyether (PE). Therefore, it is important to study its properties and behavior under different test conditions. This study investigated the dimensional stability of 5 VPES consistencies when stored for up to 2 weeks, with and without using a standard disinfection procedure. MATERIALS AND METHODS 40 discs of each VPES consistency (total 200) were made using a stainless steel die and ring as described by ANSI /ADA specification No. 19. 20 discs of each material were immersed in a 2.5% buffered glutaraldehyde solution for 30 minutes. Dimensional stability measurements were calculated immediately after fabrication and repeated on the same discs after 7 and 14 days of storage. The data was analyzed using two-way ANOVA with a significance level set at α = 0.05. RESULTS The discs mean contraction was below 0.5% at all test times ranging from 0.200 ± 0.014 to 0.325 ± 0.007. Repeated measures ANOVA showed a statistically significant difference after 2-week storage between the disinfected and non-disinfected groups ( P CONCLUSION The dimensional changes of VPES impression discs after disinfection and prolonged storage complied with ANSI/ADA standard. The tested VPES impression materials were dimensionally stable for clinical use after disinfection for 30 minutes in glutaraldehyde and storage for up to 2 weeks.
机译:用途乙烯基聚醚有机硅(VPES)与其他弹性印模材料的成分不同,因为它结合了乙烯基聚硅氧烷(VPS)和聚醚(PE)。因此,研究其在不同测试条件下的特性和行为非常重要。这项研究调查了在不使用标准消毒程序的情况下,最多存放2周时5种VPES稠度的尺寸稳定性。材料和方法按照ANSI / ADA规范No.19的说明,使用不锈钢模具和环制作40个每种VPES浓度的圆盘(总计200个),将每种材料的20个圆盘浸入2.5%的戊二醛缓冲溶液中30分钟。 。在制造后立即计算尺寸稳定性,并在存放7天和14天后在同一光盘上重复进行。使用双向ANOVA分析数据,显着性水平设置为α= 0.05。结果椎间盘的平均收缩率在0.200±0.014至0.325±0.007的所有测试时间内均低于0.5%。重复测量的方差分析显示,消毒组和未消毒组在保存2周后有统计学差异(P结论消毒后和长时间保存后VPES压印盘的尺寸变化符合ANSI / ADA标准。在戊二醛中消毒30分钟后可稳定用于临床,并保存长达2周。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号