摘要

目的 探讨反复熔铸对钴铬烤瓷合金力学性能的影响.方法 钴铬烤瓷合金经过单纯反复熔铸3次后,用拉伸实验对各代试件的拉伸强度、0.2%屈服强度、延伸率进行比较;用弯曲实验对各代试件的弯曲强度、弯曲模量进行比较;用硬度实验对各代试件的维氏硬度值进行比较.结果 经过不同熔铸次数的钴铬烤瓷合金的拉伸强度、0.2%屈服强度、延伸率、弯曲强度、弯曲模量及维氏硬度值差异均无统计学意义.结论 钴铬烤瓷合金至少可以反复熔铸3次而不引起力学性能的下降.%Objective To study the mechanical properties of Co-Cr ceramic alloy after recasts. Methods Co-Cr ceramic alloy cast samples were prepared and recast for 3 times without adding any new Co-Cr ceramic alloy. The tensile strength, 0.2% yield strength, percentage of elongation, flexural strength, flexural modulus and Vickers hardness of each specimen were measured. Results Being east for different times, the Co-Cr ceramic alloy showed no significant differences on their tensile strength, 0.2% yield strength, percentage of elongation, flexural strength, flexural modulus and Vickers hardness. Conclusion Co-Cr ceramic alloy can be recast for 3 times at least, without decrease of the mechanical properties.

著录项

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号