This article by adding different concentrations of stabilizers,different levels of nano powder,adjust the different mixing time,at different concentrations,orthogonal experiment and,ultimately,a best Ni - P - TiO2( nanometer ) composite plating Nickel formula. The formula is:thiourea 2mg· L-1;nanometer TiO2 2g· L-1;mixing time interval 2min;pH value of 5. 0. This recipe bath stability,long life,fast deposition rate can be used for production practices.%通过添加不同浓度的稳定剂,不同含量的纳米粉,调整不同的搅拌时间,在不同的浓度下,进行正交试验,最终获得一套最佳的Ni-P-TiO2(纳米)化学复合镀镍配方。其配方为:硫脲2mg·L-1;纳米 TiO22g·L-1;搅拌时间间隔2min;pH值5.0。此配方镀液稳定,使用寿命长,镀速快,可用于生产实践。