摘要

新疆某铁矿选厂采用弱磁选-强磁选-重选工艺处理低品位混合型铁矿石,虽然铁精矿品位可达65%,但回收率仅50%左右.为此采用干式预选-弱磁选-强磁选-反浮选工艺对该矿石进行了旨在提高回收率的选矿试验.试验结果表明,干式预选可先抛弃占原矿约20%的废石,最终精矿铁品位为65.25%,回收率达69.28%,比现场生产指标提高了约19个百分点.%The process of low intensity magnetic separation-high intensity magnetic separation-gravity separation was adopted to treat the low-grade mixing iron ore of Xinjiang Provicne, by which the iron concentrate grade reached 65% , but the recovery was only about 50%. Therefore, in order to improve the recovery, the beneficiation tests were carried out by the process of dry pre-concentration, low intensity magnetic separation-high intensity magnetic separation-reverse flotation. The test results showed that about 20% of the waste rocks were removed by the dry pre-concentration firstly. Then, the final concentrate graded at 65.25% with the recovery rate of 69. 28% , which is higher by about 19% than that of on-site production.

著录项

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号