刚果(金)Kamoa微细粒铜矿石浮选试验

     

摘要

Aiming at characteristics of complex dissemination and uneven particles size dissemination of copper minerals from Kamoa, Democratic Republic of Congo, beneficiation experiment was conducted by stage grinding stage separation process. With lime as a pH regulator,Cytec Aero 3894 +Cytec Aero 5100(mass ratio of 2 ∶ 1) as combined collector,and Cy-tec F507 as foamer,at grinding fineness of 85% passing 0. 053 mm,through one roughing and two flash-cleaning,scavenging rough concentrate,flash-cleaning tailings and the+0. 053 mm coarse fraction of scavenging tailings combined and then regrind-ing to fineness of 80% passing 0. 01 mm,through two scavenger-cleaning process,then a combined concentrate of flash-clean-ing and scavenger-cleaning with 48. 57% Cu and recovery of 88. 34% was obtained.%针对刚果(金) Kamoa铜矿石中铜矿物嵌布粒度粗细极不均匀、嵌布关系复杂的特点,采用阶段磨选工艺进行了选矿试验。试验以石灰为矿浆pH值调整剂,Cytec Aero 3894+Cytec Aero 5100(质量配合比为2∶1)为组合捕收剂,Cytec F507为起泡剂,在磨矿细度为-0.053 mm占85%情况下,采用1次粗选2次快速精选,快速精选尾矿、扫选精矿、扫选尾矿中的+0.053 mm粒级合并再磨至-0.01 mm占80%后,进行2次扫精选流程处理矿石,快速精选精矿与扫精选精矿合并的精矿铜品位为48.57%、回收率为88.34%。

著录项

  • 来源
    《金属矿山》|2016年第9期|100-102|共3页
  • 作者

    鲁军;

  • 作者单位

    低品位难处理黄金资源综合利用国家重点实验室;

    福建 龙岩364200;

    紫金矿业集团股份有限公司;

    福建 龙岩364200;

    北京科技大学土木与环境工程学院;

    北京100083;

  • 原文格式 PDF
  • 正文语种 chi
  • 中图分类 TD923+.7;
  • 关键词

    微细粒铜矿石; 快速精选; 中矿再磨选;

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号