将干燥的块状煤泥研磨至不同粒度的煤粉,与造纸黑液按一定比例配制成水煤浆,考察其综合性能指标.当黑液添加量为7.2%,煤粉粒度小于160目时,制备的水煤浆浓度为67.44%,流动性为A级,稳定性达到20 d保持良好.改变黑液的pH值,研究其配制的水煤浆,发现废液pH对水煤浆的成浆性没有太大的影响.由于造纸黑液中含有大量有机质,因此还可提高同等条件下水煤浆的燃烧热值.利用GB 213-87测定所制备水煤浆的恒容高位发热量为21.63 MJ/kg,低位发热量为15 MJ/kg.%Based on the character of high ash and large amount of moisture in the coal slime, and hard to handle of the actual situation of black liquor for paper making which contains abundant organism, it is an useful attempt by using dry method to make water coal mixture both as the raw material. The water coal mixture is made from powdered coal of different particle size which abrading the dry nubby coal slime and black liquor for paper making by a certain percentage in order to research the indicator of comprehensive performance. When the add content of black liquid is 7. 2% and the particle size of powdered coal is less than 160 mesh, the concentration of water coal mixture is 67. 44% , liquidity will be A grade and the stability will retain almost 20 d in good condition. The experiment results indicate that the pH value of waste almost has no effect on the slurry-ability of water coal slime if the pH value of black liquid is changed to research the prepared of water coal slime. Due to the black liquid of paper making contains large amount of or ganic matter, therefore, it can also improve the combustion heat value of water coal slime under the same conditions. The constant-volume high heat of the prepared water coal slime is 21. 63 MJ/kg, low heat is 15 MJ/kg, which is measured by GB 213-87.

著录项

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号