The goal of this thesis is to develop more effective quantitative procedures to evaluate the stability of deteriorated metal culverts and a better understanding of the deteriorated culverts' behaviour through non-destructive testing, full scale experiments and numerical analyses. First, three design cases were examined using numerical analysis to study the effects of corrosion, burial depth and staged construction on the capacity of deteriorated steel culverts. Then, a method to measure the remaining wall thickness of two 1.8 m diameter corroded metal culverts using ultrasonic device was developed. Both culverts were then buried in the test pit at Queen's University and tested under nominal and working vehicle loads at 0.9m cover and 0.6m cover. The more heavily corroded structure (CSP1) was tested up to its ultimate limit state, inducing local bending across the crown, as well as local buckling of the remnants of the corrugated steel wall between perforations at the haunches. The results suggest that the single axle pads interact to influence the culvert's behaviour despite the shallow cover used in these experiments. CSP1 was able to carry the working load and did not fail until reaching 340 kN, which was equal to 90% of the fully factored load. The experiment suggests that less deteriorated metal culverts (as compared to CSP1) may have the required capacity. Two finite element packages, CANDE and ABAQUS, were used to perform the numerical investigation and the AASHTO and CHBDC approaches were then used to calculate the thrust force in the culverts. Although the numerical analysis produced conservative values for the thrust forces, it failed to capture the non-linear behaviour of both specimens in the experiments. Both the AASHTO and the CHBDC approaches produced unconservative thrust forces compared to experimental results while numerical analysis using Moore's spreading factor produced the most conservative results in terms of thrust. The analysis suggests that CANDE could be used to predict thrust forces in less deteriorated metal culverts. A procedure to assess the stability of deteriorated corrugated metal culverts based on quantitative data was developed using the numerical analysis and experimental results.
机译:本文的目的是开发更有效的定量程序,以评估退化的金属涵洞的稳定性,并通过无损检测,全面实验和数值分析更好地了解退化的涵洞的行为。首先,使用数值分析研究了三个设计案例,以研究腐蚀,埋深和分阶段施工对退化钢涵的承载力的影响。然后,开发了一种使用超声波装置测量两个直径为1.8 m的腐蚀金属涵洞的剩余壁厚的方法。然后将两个涵洞都埋在皇后大学的测试坑中,并在0.9m覆盖和0.6m覆盖的名义和工作车辆载荷下进行测试。经过更严重腐蚀的结构(CSP1)进行了测试,直至达到极限极限状态,引起了整个冠部的局部弯曲,以及在弯头处的穿孔之间的波纹状钢壁残余物局部屈曲。结果表明,尽管在这些实验中使用了较浅的覆盖层,但单轴瓦相互作用也会影响涵洞的行为。 CSP1能够承受工作负载,直到达到340 kN才失效,这等于完全分解负载的90%。实验表明,退化的金属涵洞(与CSP1相比)可能具有所需的容量。使用两个有限元程序包CANDE和ABAQUS进行数值研究,然后使用AASHTO和CHBDC方法计算涵洞中的推力。尽管数值分析产生了推力的保守值,但未能捕获实验中两个样本的非线性行为。与实验结果相比,AASHTO方法和CHBDC方法都产生了非保守的推力,而使用Moore扩展因子的数值分析在推力方面产生了最保守的结果。分析表明,CANDE可用于预测退化程度较小的金属涵洞的推力。利用数值分析和实验结果,开发了一种基于定量数据评估退化波纹金属涵洞稳定性的方法。

著录项

  • 作者

    Mai, Van Thien.;

  • 作者单位

    Queen's University (Canada).;

  • 授予单位 Queen's University (Canada).;
  • 学科 Engineering Civil.
  • 学位 M.S.
  • 年度 2013
  • 页码 234 p.
  • 总页数 234
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号