Orthotropic Deck Wear Surface System Selection Lions Gate Bridge North Approach Viaduct, Vancouver BC

机译:正交各向异性甲板磨损表面系统的选择狮子门大桥北进桥高架桥,温哥华

获取原文

摘要

The paper presents the wear surface replacement options analysis methodology that was used to select the resurfacing system for the Lions Gate Bridge North Approach Viaduct in Vancouver British Columbia. The objective was to select the surfacing system that presents the best combination of performance and value. Lions Gate was opened to traffic in 1938. The bridge carries three traffic lanes, the centre lane is a counterflow (reversible) lane whereby two lanes are open to traffic in one direction at any given time, and a single lane is open in the opposite direction. The original bridge deck of the North Viaduct was replaced in 1975 with an orthotropic steel deck. The orthotropic deck was first surfaced with epoxy asphalt concrete and has since been resurfaced several times with bituminous asphalt concrete, most recently in 2001. A list was prepared of potential surfacing systems that have been used on orthotropic decks. The surfacing systems evaluated included: Bolidt ZOK; Epoxy Asphalt Concrete; Gussaspha Polyester Concrete; Polymer Modified Asphalt Concrete; Rosphalt 50; and Trinidad Lake Asphalt. An estimated construction cost and life cycle cost was prepared for each alternative wear surface system. Each system was then evaluated based on a number of weighted criteria. The paper presents the ranking for each material, and then presents the outcome in terms of the highest ranking wear surface systems.
机译:本文介绍了磨损表面更换选项分析方法,该方法用于选择不列颠哥伦比亚省温哥华市的狮门大桥北引桥高架桥。目的是选择表现出性能和价值的最佳组合的表面处理系统。狮子门(Lions Gate)于1938年开放通行。该桥载有3条行车线,中央车道是逆流(可逆)车道,其中两条车道在任何给定时间向一个方向开放,而一条车道在对面开放方向。北高架桥的原始桥面板在1975年被正交异性钢桥面板所取代。正交异性甲板首先用环氧沥青混凝土进行表面处理,此后又多次用沥青沥青混凝土进行了表面重新铺砌,最近一次是在2001年。列出了已在正交异性甲板上使用的潜在铺面系统清单。评估的表面处理系统包括:Bolidt ZOK;环氧沥青混凝土; Gussasphalt;聚酯混凝土;聚合物改性沥青混凝土;罗斯福50;和特立尼达湖沥青。为每个替代磨损表面系统准备了估计的建筑成本和生命周期成本。然后根据许多加权标准评估每个系统。本文介绍了每种材料的等级,然后以最高等级的磨损表面系统给出了结果。

著录项

相似文献

  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号