There is a tendency in anode baking furnaces to reduce the thickness of the flue walls; the main purpose of this reduction is to increase the size of anodes (spacing). If the thickness of the flue wall is reduced with 10 % the life time of the flue wall will be reduced by up to 20%. In other cases the height of the flue walls will increase, so the refractory has to withstand more severe conditions and the life time will be reduced as well. To overcome these problems, Gouda Vuurvast developed a new generation of bricks with reduced permeability and low alkali content. The lower permeability prevents alkali and fluoride containing gasses to penetrate in the brick. The lower alkali content gives a better starting point of the new flue walls and more "penetrated" alkali can be absorbed by these bricks before the flue walls will collapse. The lower permeability and the lower alkali content will result in a longer life time of the refractories. A number of field tests with this new generation of LP 50S bricks are running.
机译:阳极烘烤炉有减小烟道壁厚度的趋势。这种减少的主要目的是增加阳极的尺寸(间距)。如果将烟道壁的厚度减少10%,则烟道壁的使用寿命将减少多达20%。在其他情况下,烟道壁的高度会增加,因此耐火材料必须承受更严酷的条件,使用寿命也会缩短。为了克服这些问题,Gouda Vuurvast开发了新一代渗透性降低且碱含量低的砖。较低的渗透率可防止含碱和氟化物的气体渗透到砖中。较低的碱含量为新烟道壁提供了更好的起点,并且在烟道壁倒塌之前,这些砖可以吸收更多的“渗透”碱。较低的渗透率和较低的碱含量将导致耐火材料的使用寿命更长。新一代LP 50S砖正在进行许多现场测试。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号