A study was conducted to identify the environmental influence on fatigue crack growth behavior of three high strength steels: AerMet 100, 300M, and 4340. These steels were subjected to fatigue tests under constant amplitude loading of frequency 10 Hz and stress ratios R = 0.1 and 0.9, in vacuum, air, and 3.5 % NaCl solution. The fatigue crack growth was characterized with two driving force parameters, stress intensity range, ΔK, and maximum stress intensity, K_(max). Especially, the variation of fatigue crack growth per time, da/dt, with K_(max) in 3.5 % NaCl solution was evaluated with respect to R, environment, and threshold stress intensity for environmentally assisted cracking (EAC), K_(IEAC). In addition, the environmental influence on fatigue crack growth was examined with the fractographic features and trajectory path, drawn with the limiting values of ΔK and K_(max), ΔK~* and K_(max)~*.
机译:进行了一项研究,以确定环境对三种高强度钢:AerMet 100、300M和4340的疲劳裂纹扩展行为的影响。这些钢在频率为10 Hz的恒定振幅载荷和应力比R = 0.1的情况下经受了疲劳测试。 0.9,在真空,空气和3.5%NaCl溶液中。疲劳裂纹扩展的特征在于两个驱动力参数,即应力强度范围ΔK和最大应力强度K_(max)。尤其是,针对R,环境和环境辅助裂纹(EAC)的阈值应力强度K_(IEAC),评估了3.5%NaCl溶液中疲劳裂纹扩展随时间的发展da / dt随K_(max)的变化。 。另外,利用分形特征和轨迹轨迹,考察了环境对疲劳裂纹扩展的影响,并以ΔK和K_(max),ΔK〜*和K_(max)〜*作为极限值。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号