Sensitivity evolution of NEPE propellant during ageing

机译:NEPE推进剂老化过程中的敏感性演变

获取原文

摘要

With high level of output energy, NEPE (Nitrate Ester Plasticized Polyether) propellant has attracted considerable attention. However, it also suffers from ageing problems due to the decomposition of the nitrate ester plasticizer and production of NO_2. which results in further decomposition of polymer substrate. Besides aroused mechanical problems, this process can also lead to a safety problem. To investigate the sensitivity evolution of NEPE propellant during storage life, variations of 5-second explosion temperature, volume of released gas in vacuum stable test, characteristic drop height, 50% explosion pressure and static spark energy with accelerated ageing time were monitored and the results were treated with fuzzy comprehensive evaluation (FCE) method. A tendency of increasing sensitivity was noticed. The results show that after approximately 36-45 days' ageing under 70 ℃, the sensitivity went through a step change. The pores created by the integrity compromise of polymer structure during ageing accounts for the sensitivity evolution of NEPE propellant. As such, the discovery of more effective stabilizer is urged to improve the storage safety of NEPE propellant.
机译:凭借高水平的输出能量,NEPE(硝酸酯增塑聚醚)推进剂备受关注。然而,由于硝酸酯增塑剂的分解和NO_2的产生,它也遭受老化问题。这导致聚合物底物进一步分解。除了引起机械问题外,此过程还会导致安全问题。为了研究NEPE推进剂在储存期间的敏感性演变,监测了5秒爆炸温度,在真空稳定测试中释放的气体量,特征降落高度,50%爆炸压力和具有加速老化时间的静态火花能量的变化,并得出了结果用模糊综合评价法(FCE)进行治疗。注意到灵敏度增加的趋势。结果表明,在70℃下约36-45天老化后,灵敏度发生了阶跃变化。在老化过程中,由于聚合物结构的完整性受损而产生的孔可解释NEPE推进剂的敏感性演变。因此,敦促发现更有效的稳定剂以改善NEPE推进剂的储存安全性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号