There are two eutectic systems in the Al_2O_3-Y_2O_3 system: one is the Al_2O_3-YAG equilibrium eutectic system and the other is the Al_2O_3-YAP metastable eutectic system. Heating the Al_2O_3-YAP metastable eutectic structure up to temperatures above the metastable eutectic temperature but below the equilibrium eutectic temperature produced the undercooled melt. Solidification in the equilibrium path immediately followed the undercooled melt formation. The solidification in the equilibrium path along with the melting of the metastable eutectic structure resulted in a fine and uniform equilibrium eutectic structure. This paper demonstrates the shape casting by using the undercooled melt formation.
机译:Al_2O_3-Y_2O_3系统中有两个共晶体系:一个是Al_2O_3-YAG平衡共晶体系,另一个是Al_2O_3-YAP亚稳共晶体系。将Al_2O_3-YAP亚稳共晶结构加热到高于亚稳共晶温度但低于平衡共晶温度的温度会产生过冷熔体。平衡路径中的凝固紧随过冷熔体形成之后。在平衡路径中的凝固以及亚稳态共晶结构的熔化导致了精细而均匀的平衡共晶结构。本文演示了使用过冷熔体的形状铸造。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号