The key to preparing high-purity cobalt is purifying of cobalt solution. Cobalt sulfate solution was refined by PC88A levextrel Resins which produced from HPD-100 type of ethylene benzene -divinylbenzene porous adsorption resin and PC88A extractant. The results indicate that under the condition which the solvent impregnated resins containing PC88A is 55% in Φ>65 mm ×700mm chromatography column, extraction pH value is 3.7, buffer elution pH value is 2.9, velocity of flow isl~1.5 chromatography column volume/h, when solution volume is three times of column volume, stripping solution is collected and stripping by pH 1.0 hydrochloric acid. The high purity cobalt chloride solution is obtained. Removing organic impurity form cobalt chloride solution and concentrating, the high purity cobalt which obtained by electrolyze the cobalt chloride solution is tested by GDMS. The results indicate that the total impurity of twenty elements is less than 10 ppm.
机译:制备高纯度钴的键是纯化钴溶液。通过HPD-100型乙烯苯-Divinylen苯多孔吸附树脂和PC88A萃取剂制备硫酸钴溶液。结果表明,在含有Pc88a的溶剂浸渍树脂在φ> 65mm×700mm色谱柱中为55%的情况下,提取pH值为3.7,缓冲洗脱pH值为2.9,流动的速度为〜1.5色谱柱体积/ h,当溶液体积是柱体积的三次时,收集汽提溶液并通过pH 1.0盐酸汽提。获得高纯度氯化钴溶液。除去有机杂质形成钴氯化物溶液并浓缩,通过GDMS测试通过电解氯化钴溶液而获得的高纯度钴。结果表明,二十元素的总杂质小于10ppm。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号