Previous research indicated that the expansion property of MgO-type expansive agent (MEA) strongly depended on the amount. However, the quantitative effect of amount on expansion property of MEA has not been clearly demonstrated. In the present the expansion value of cement paste with 3%, 4%, 5% and 6% MEA calcinated at 850°C and 1200 °C, and then relative expansion value was introduced to investigated the relationship between the mount and expansion of MEA. The results indicated The relative expansion of MEA calcinated at 850°C was relative invariant to curing temperature and proportional increased with the amount ratio. The relative expansion of MEA calcinated at 1200°C proportional increased with curing age, and the increasing rate rose with the amount ratio of MEA and curing temperature.
机译:以前的研究表明,MgO型膨胀剂(MEA)的扩展性能强烈依赖于金额。 然而,未清楚地证明了MEA扩增属性对膨胀性质的定量效果。 在本处于850°C和1200°C的3%,4%,5%和6%MEA的水泥浆料的膨胀值,然后引入了相对膨胀值来研究MEA的安装和扩展之间的关系 。 结果表明,在850℃下煅烧的MEA的相对膨胀是固化温度的相对不变,随比比例增加。 MEA的相对膨胀在1200℃下煅烧成比例随固化年龄而增加,并且随着MEA和固化温度的量比,增加的速率升高。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号