The Effect of Clamshell Ash Substitution to the Mechanical Properties of Concrete

机译:蛤壳灰烬取代在混凝土机械性能下的影响

获取原文

摘要

Concrete is the main material for construction that is widely used throughout the world.The more widespread use of concrete and the increasing scale of development also shows more and more concrete needs in the future.The era development of this rapid globalization era has resulted in the increasing number of used goods/waste whose existence can be a problem for life,one of which is the presence of clamshell ash.For this reason,many things have been done in order to recycle to overcome the problem of the existence of this waste.One of them is that clamshell ash can be used as a substitute for cement in a concrete mixture.This research uses clamshell ash and lime with variations of 0%,5%,10%,15%,and 20% from the use of cement.The substitution of clamshell ash and lime affects the strength of the concrete.There are an increase in slump value with the substitution of clamshell ash by 8,9,11,13,14 and lime substitution by 8,8,5,10,12,13.There are a decrease in compressive strength on the substitution of clamshell ash by 89.18%,74.09%,67.87%,64.92% of normal concrete and compressive strength on lime substitution by 69.84%,58.53%,57.05 %,55.82% of normal concrete.There are a decrease in split tensile strength in the substitution of clamshell ash by 95.96%,92.3%,81.7%,75.8% of normal concrete and split tensile strength on lime substitution by 87.93%,81.33%,65,92%,48.37% of normal concrete.
机译:混凝土是全球广泛使用的结构的主要材料。更广泛使用的混凝土和日益发展规模的发展也展示了未来越来越多的具体需求。这种快速全球化时代的时代的发展也导致了越来越多的使用商品/浪费,其存在可能是生命的问题,其中一个是蛤壳灰的存在。对于这个原因,已经完成了许多事情,以便回收克服这种废物存在的问题。其中一个是蛤壳灰可以用作混凝土混合物中的水泥的替代品。本研究使用水泥使用0%,5%,10%,15%和20%的蛤壳灰和石灰。 。蛤壳灰和石灰的替代力影响了混凝土的强度。随着8,9,11,13,14和石灰替代,克拉姆谢灰替代坍落度的坍落度增加了8,8,5,10, 12,13. S的抗压强度降低蛤壳粉剂的Ubstitut原液89.18%,74.09%,67.87%,64.92%的常规混凝土和抗压强度替换为69.84%,58.53%,58.53%,57.05%,55.82%的正常混凝土。分裂拉伸强度降低将ClamShell灰分替代为95.96%,92.3%,81.7%,75.8%的正常混凝土和分裂拉伸强度的液体替代力87.93%,81.33%,65,92%,48.37%的正常混凝土。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号