Osteocompatibility of photopolymerizable anhydride networks

机译:可光聚合的酸酐网络的骨质组成性

获取原文
获取外文期刊封面目录资料

摘要

A new family of polyanhydrides has been developed which can be cured photochemically to produce degradable networks. These degradable polyanhydride networks can be useful in orthopedics as bone cements and for drug delivery. This system, which is a semi-interpenetrating network (semi-IPN), has been evaluated for tissue compatibility in subcutaneous sites in rats and shown to undergo degradation by surface erosion. It was observed that the inflammatory response to the semi-IPN implants was minimal at both short (3, 6 weeks) and long (28 weeks) time points and the fibrotic response was large4ly absent throughout the duration of this study. Furthermore, excellent tissue infiltration and integration with good neovascularization was observed around the semi-IPN implants. The osteocompatibility and osteoconductive properties of this system have been evaluated in a longitudinal defect model in the articular surface of the distal femur in adult rabbits. This study compared the semi-IPN implants to control groups consisting of unfilled defects and PLA implants. Histological evaluation (H&E and Trichrome Masson staining) of the implant site revealted that the semi-IPN implant is osteocompatible and well tolerated by the surrounding cancellous bone and marrow constituents. The tissue reaction to the implant is characterized by an ingrowth of vascularized connective tissue and a mild fibrous capsule. Furthermore, partial to complete closure of the articular surface with fibrocartilage and fibrous tissue was observed in all experimentla animals containing the semi-IPN polymer implants.
机译:已经开发了一种新的多烷酰亚醇家族,其可以采用光化学地固化以产生可降解网络。这些可降解的多烷氢化物网络可用于骨科和药物递送的骨科。该系统是半渗透网络(半IPN)的系统,已经评估了大鼠皮下位点的组织相容性,并被证明通过表面侵蚀进行降解。观察到,对于SEMI-IPN植入物的炎症反应在短(3,6周)和长(28周)时间点最小,并且在整个研究期间,纤维化反应大4次缺席。此外,在半IPN植入物周围观察到优异的组织渗透和与良好的新血管形成的整合。该系统的骨相干性和骨质变性和骨导电性能已经在成人兔子远端股骨的关节表面中的纵向缺陷模型中评估。本研究将半IPN植入物与未填充缺陷和PLA植入组成的控制组进行比较。植入部位的组织学评估(H&E和richrome Masson染色)揭示了半IPN植入物是由周围的松质骨和骨髓成分溶于骨质组织和良好的耐受性。对植入物的组织反应的特征在于血管化结缔组织和轻度纤维状胶囊的成长。此外,在含有半IPN聚合物植入物的所有实验动物的所有实验动物中,观察到局部地完成具有纤维纤维轴和纤维组织的关节表面。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号