filler is one of the ingredients functioning as a filler of ribs from a paved mixture.In a flexible pavement structure,the surface layer is the most upper part of the pavement which acts to hold the wheel load and also as a dense layer of water to protect the required road body,with a minimum thickness of 4 cm.This research was conducted by experimental method aiming to know the highest stability value using volcanic ash deposits as a substitute for cement in the filler.The deposits of volcanic ash used are 0%,25%,50%,75% and 100% of the filler weight.The specimen material consists of several types,namely Marshall,PRD,IP,and GMM specimens.Concrete asphalt mixture is designed on the basis of the Marshall method.The results show that the volcanic deposit content is 0% with a stability value of 1133 kg,15% with 1151 kg stability value,30% with 1076 kg stability value,50% with 1056 kg stability value,70% with 1048 kg stability value,85% with 1047 kg stability value and 100% with 1121 kg stability value.From these variations,the highest stability value is found in 15% volcanic ash deposition with 1151kg.
机译:填料是从铺设的混合物中作为肋的填料的成分之一。在柔性的路面结构中,表面层是路面的最上部,其用来保持车轮载荷和作为致密的水层保护所需的道路体,最小厚度为4cm。通过实验方法进行了研究,旨在利用火山灰沉积物作为填料中的水泥替代品的最高稳定性值进行。使用的火山灰的沉积物为0% ,25%,50%,75%和100%的填料重量。标本材料由几种类型,即马歇尔,PRD,IP和GMM样本组成。基于Marshall方法设计的沥青混合物。结果表明,火山沉积含量为0%,稳定值1133千克,15%,具有1151千克稳定值,1076千克稳定值,50%,1056千克稳定值,70%,具有1048千克稳定值,为1048千克稳定值, 85%,1047千克稳定值,100%,1121千克能力值。从这些变化中,最高稳定性值在15%的火山灰沉积中找到1151kg。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号