Ion Nitriding of Steels in a System with a Thermionic Gas Plasma Source

机译:热离子等离子体源的系统中钢的离子氮化

获取原文

摘要

A study has been made into the method of ion nitriding of tool steels in the nitrogen plasma of arc discharge with a thermionic cathode. It is found that ion nitriding with a thermionic source of nitrogen plasma causes a considerably lower hydrogenation of steels than in the cases of gas nitriding in the presence of ammonia or ion nitriding in nitrogen-hydrogen mixtures in a glow discharge. The nitrogen concentration in subsurface layers of nitrided steels is 21 to 27 at.%. The process of ion nitriding lasted for 2 to 4 hours. After the process, the microhardness of carbon steel and alloyed steel surfaces increases by factors of 2 to 5. The greatest thickness of the hardened layer reaches 150 μm.
机译:用热电偶阴极对电弧放电氮等离子体进行离子氮化的方法。 发现与氮等离子体的热离子源的离子氮化导致钢的氢化比在氨氢混合物存在下氮气存在的氮气存在下的气体氮气的情况下。 氮化钢的地下层中的氮浓度为21至27.%。 离子氮化的过程持续2至4小时。 在该过程之后,碳钢和合金钢表面的显微硬度随2至5的因素而增加。硬化层的最大厚度达到150μm。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号