Anodic oxidation of aluminum alloy in a ternary solution of SAS (sulfuric, adipic and oxalic acids) was carried out in order to obtain the aluminum oxide layer (Al_2O_3) and Al_2O_3 with inorganic fullerene-like tungsten disulfide (IF-WS_2) named in article as Al_2O_3/IF-WS_2. The micro-hardness, thickness, geometric structure of the surface (SGP) and the microstructures of Al_2O_3 and Al_2O_3/IF-WS_2 were investigated. The influence of electrolysis time, temperature and type of electrolyte on the micro-hardness of coatings was studied using the Taguchi statistical method. A L2 orthogonal array with the three main factors of control at two levels each was studied. Signal-to-noise ratio showed that the great influence of temperature on micro-hardness. The optimized electrolysis conditions were defined.
机译:进行SAS(硫酸,己二酸和草酸)的三元溶液中铝合金的阳极氧化,以获得在文章中命名的无机富勒烯样钨(IF-WS_2)的氧化铝层(Al_2O_3)和Al_2O_3 作为al_2o_3 / if-ws_2。 研究了表面(SGP)的微硬度,厚度,几何结构和Al_2O_3和Al_2O_3 / IF-WS_2的微观结构。 使用TAGUCHI统计方法研究了电解时间,电解质对电解质对涂层微硬度的影响。 研究了L2正交阵列,每个阵列都有三个主要控制的两个级别。 信噪比表明,温度对微硬度的影响很大。 定义了优化的电解条件。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号