Compared activity and stability of three Ni-silica catalysts for methane bi- and dry reforming

机译:三种硅胶催化剂的比较甲烷二氧化硅催化剂的活性和稳定性

获取原文

摘要

A low weight % of Ni (5 wt %) and the two solvents technique of deposition are used to obtain well-dispersed Ni-species (either particles or species dispersed on the silica surface) and avoid the formation of large particles on three silicas SBA-15, Aerosil 300 and diatoms MN3. Stability tests at 650°C for valorization of methane obtained from natural or shale gas: methane dry reforming and at 800°C for bireforming are compared. For bireforming (steady state, 800°C, 10 h, CH/CO/HO 1:0.4:0.8, 62,700 ml·g·h), an unexpected stability of Ni/Aerosil silica is observed and tentatively associated with the pretreatment applied to silica.
机译:低重量%的Ni(5wt%)和两种沉积溶剂技术用于获得井分散的Ni型(分散在二氧化硅表面上的颗粒或物种),并避免在三个硅SBA上形成大颗粒-15,Aerosil 300和硅藻Mn3。 650℃的稳定性试验用于自然或页岩气中获得的甲烷的储存:比较甲烷干重整和800℃的生物形成。对于生物形成(稳态,800°C,10 H,CH / CO / HO 1:0.4:0.8,62,700mL·G·H),观察到Ni / Aerosil二氧化硅的意外稳定性,并暂时与应用于的预处理相关二氧化硅。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号