The effect of MgO, CNT, TiO_2 addition on the structural and transport properties of Bi_(1.6)Pb_(0.4)Sr_2Ca_2Cu_3O_8 superconducting samples have been investigated. The samples were prepared by solid-state method and recurrent sintering. The samples were characterized by x-ray diffraction (XRD), scanning electron microscopy, and electrical resistivity measurement. The critical superconductivity transition temperature (Tc) of MgO, CNT, TiO_2 addition were found to be lower than the pure sample. T_(c-onset) was found 121.5 K; 117.5 K; 120.8 K; 120.1 K with broad transition 15.4 K; 15.8 K; 22 K; 46.8 K for pure BPSCCO sample and MgO, CNT, TiO_2 addition samples, respectively. XRD analysis showed that the decrease of the volume fraction Bi-2223 and increase Bi-2212 phase with addition MgO, CNT, and TiO_2. Recurrent sintering increased Tc and narrowed transition temperature.
机译:研究了MgO,CNT,TiO_2的作用对Bi_(1.6)Pb_(0.4)SR_2Ca_2Cu_3O_8超导样品的结构和传输性能进行了添加。通过固态方法和复发烧结制备样品。通过X射线衍射(XRD),扫描电子显微镜和电阻率测量表征样品。发现MgO,CNT,TiO_2添加的临界超导转变温度(Tc)低于纯样品。发现了121.5 k的t_(c-onset); 117.5 k; 120.8 k; 120.1 k,具有宽过渡15.4 k; 15.8 k; 22 k; 46.8 k用于纯BPSCCO样品和MgO,CNT,TiO_2添加样品。 XRD分析表明,体积分数BI-2223的降低和增加Bi-2212相加入MgO,CNT和TiO_2。复发烧结增加了Tc和变窄的过渡温度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号