Unique Hydrometallurgical Process for Copper-Anode Slime Treatment at Saganoseki Smelter and Refinery

机译:Saganoseki冶炼厂和炼油厂的铜阳极粘液处理独特的湿法冶金工艺

获取原文

摘要

Saganoseki Smelter and Refinery of Pan Pacific Copper Co., Ltd. started treating copper anode slimes using a unique hydrometallurgical process in chloride media in 1997. The process comprises the following stages, decopperizing, wet chlorination, solvent extraction for gold, silver chloride reduction, and separate reduction stages that treat the gold extraction raffinate with sulfur dioxide gas. Precious metals and rare metals in the copper anode slimes are dissolved in an aqueous solution of hydrochloric acid by oxidative leaching, which is termed wet chlorination. Gold is efficiently extracted from the chlorination liquor by dibutyl carbitol in the solvent extraction stage. Gold is reduced by oxalic acid from gold-loaded dibutyl carbitol and recovered as gold powder. The gold powder is cast directly into granules or ingots of more than 99.99% purity without electrorefining. Selenium is recovered as a selenium residue by reduction with sulfur dioxide gas and refined through vacuum distillation. The plant was designed to process 132 tonnes of copper anode slimes per month and has a current capacity of 206 tonnes per month due to several enhancements. Compared with the conventional process, the hydrometallurgical process described here provides some advantages, in particular, a higher product quality, shorter gold-retention time, and reduction in environmental load.
机译:泛太平洋铜有限公司的Saganoseki冶炼厂和炼油厂在1997年开始使用独特的湿法冶金工艺处理铜阳极粘性。该方法包括以下阶段,解吸,湿氯化,黄金溶剂萃取,减少氯化银,并单独减少用二氧化硫气体处理金提取萃取液。通过氧化浸出溶解铜阳极沉积物中的贵金属和稀有金属通过氧化浸出溶解在盐酸水溶液中,其被称为湿氯化。在溶剂萃取阶段通过二丁基水溶液从氯化液中有效地提取金。通过来自镀金的二丁基卡培醇的草酸降低金,并作为金粉回收。将金粉直接浇铸成颗粒或颗粒,纯度超过99.99%而无需电动。通过用二氧化硫气体还原并通过真空蒸馏来改善硒作为硒残余物回收硒。该工厂旨在处理每月132吨的铜阳极体积,由于几种增强,每月每月的目前容量为206吨。与常规过程相比,这里描述的液压冶金方法提供了一些优点,特别是更高的产品质量,较短的金保留时间和环境负荷的降低。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号