In this study, three various types of fillers; pristine multi-walled carbon nanotube (MWCNT), hydroxyl functionalized multi-walled carbon nanotube (MWCNT-OH) and carboxyl functionalized multi-walled carbon nanotube (MWCNT-COOH) were used to prepare epoxy (EP) composites via ultrasonication and casting techniques. The effect of pristine and functionalized MWCNT as well as fillers loading (0-1.0 vol%) on tensile properties of EP composites were investigated and compared. To identify the effectiveness of functional groups on the EP composites, the MWCNT, MWCNT-OH and MWCNT-COOH were compared via tensile testing. The addition of 0.4 vol% pristine MWCNT decreased the material's tensile strength and modulus by 5.13% and 2.82% respectively, while the addition of MWCNT-OH decreased the material's tensile strength by 12.80%. However, among the EP composites, the 0.4 vol% MWCNT-COOH/EP composite exhibited a 12.82% increase in tensile strength. The Young's modulus of 0.4 vol% MWCNT-OH/EP and MWCNT-COOH/EP composites were found to be significantly higher compared to unfilled EP which were approximately 15.60% and 18.54% respectively. The effect of functionalized MWCNT was supported by morphological analysis, which demonstrated an improvement in MWCNT-COOH dispersion with slightly fine agglomerates particles at 0.4 vol%.
机译:在这项研究中,三种各种类型的填料;原始多壁碳纳米管(MWCNT),羟基官能化的多壁碳纳米管(MWCNT-OH)和羧基官能化的多壁碳纳米管(MWCNT-COOH)用于制备环氧(EP)通过超声处理和铸造技术复合材料。研究了原始和官能化MWCNT以及填料加载(0-1.0体积%)对复合材料的拉伸性能的影响,并进行比较。为了鉴定EP复合材料上官能团的有效性,通过拉伸试验比较MWCNT,MWCNT-OH和MWCNT-COOH。加入0.4体积%原始MWCNT分别将材料的拉伸强度和模量降低5.13%和2.82%,同时加入MWCNT-OH将材料的拉伸强度降低12.80%。然而,在EP复合材料中,0.4体积%MWCNT-COOH / EP复合材料表现出12.82%的拉伸强度增加。与未填充的EP相比,发现杨氏模量为0.4 Vol%MWCNT-OH / EP和MWCNT-COOH / EP复合材料分别为约15.60%和18.54%。通过形态学分析支持官能化MWCNT的作用,表明MWCNT-COOH分散体具有略微精细的凝聚颗粒,颗粒为0.4体积%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号