ADSORPTIVE REMOVAL OF Pb(II) FROM AQUEOUS SOLUTION USING RAW AND WASTED LOW GRADE IRON ORE WITH PHOSPHORUS AS ADSORBENT

机译:使用原料和浪费的低等级铁矿溶液与磷作为吸附剂的吸附除去Pb(II)

获取原文

摘要

Low grade iron ore with phosphorus (LGIOWP), a raw and wasted industrial solid material was used as an adsorbent to remove Pb(II) from wastewater. The effects of initial pH value, adsorptive time, initial Pb(II) concentration, adsorptive temperature and LGIOWP dosage on the Pb(II) removal efficiency were studied. The results show that the Pb(II) removal efficiencies exceed 99.4% and Pb(II) concentrations are less than 0.30 mg/L under the conditions of pH value 7.0, adsorptive temperature 50 °C, adsorptive time 30 min, initial Pb(II) concentration 100 mg/L, particle size <0.25 mm, adsorbent dosage 5 g/L and stirring speed 260 r/min. After Pb(II) removal reaction, the Pb(II) concentrations of wastewater completely accord with the requirement of national discharge standards of pollutants from lead and zinc industries (GB 25466-2010) (TPb=0.5 mg/L) in China. Therefore, it can be concluded that LGIOWP is a new low-cost adsorbent which is suitable for the adsorption of Pb(II) from wastewater.
机译:用磷(LgiowP),原料和浪费的工业固体材料的低级铁矿石用作吸附剂,以从废水中除去Pb(II)。研究了初始pH值,吸附时间,初始PB(II)浓度,吸附温度和LgiOWP剂量对PB(II)去除效率的影响。结果表明,在pH值7.0的条件下,Pb(II)去除效率超过99.4%,Pb(II)浓度小于0.30mg / l,吸附温度50℃,吸附时间30分钟,初始Pb(II )浓度100mg / L,粒度<0.25mm,吸附剂剂量5g / L和搅拌速度260 r / min。在PB(II)除去反应后,废水的Pb(II)浓度完全符合中国铅和锌工业污染物(GB 25466-2010)(TPB = 0.5 mg / L)的国家排放标准。因此,可以得出结论,LgiOWP是一种新的低成本吸附剂,适用于废水中的Pb(II)的吸附。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号