The study focus on effect of pre-heated ceramic surface on the adhesion bond strength between geopolymer coating coating and ceramic substrates. Ceramic substrates was pre-heated at different temperature (400 °C, 600 °C, 800 °C and 1000 °C). Fly ash geopolymer coating material potential used to protect surface used in exposure conditions after sintering at high temperature. Fly ash and alkali activator (Al2O3/Na2SiO3) were mixed with 2.0 solids-to-liquid ratios to prepare geopolymer coating material at constant NaOH concentration of 12M. Adhesion test was conducted to determine the adhesion bond between ceramic substrates and fly ash coating material. The results showed the pre-heated ceramic substrates effect the adhesion bond of coating compared with untreated substrates with increasing of strength up to 20 % for temperature 600 °C.
机译:该研究侧重于预热陶瓷表面对地质聚合物涂料和陶瓷基材之间的粘合粘合强度的影响。 在不同温度(400℃,600℃,800℃和1000℃)上预热陶瓷基材。 飞灰地质聚合物涂层材料电位用于保护在高温下烧结后的暴露条件下使用的表面。 将粉煤灰和碱活化剂(Al 2 O 3 / Na 2 SiO 3)与2.0固体液体比混合,以在恒定的NaOH浓度为12m处制备地质聚合物涂料。 进行粘合试验以确定陶瓷基材和飞灰涂料之间的粘合粘合。 结果表明,预热陶瓷基材与未处理的基材相比,涂层的粘合粘合效果,其温度高达20%的强度为600℃。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号