Corrosion of 304L Stainless Steel Tube in Power Plant Condenser

机译:304L不锈钢管在发电厂冷凝器中的腐蚀

获取原文

摘要

Before being put to use, a new condenser of 600 MW unit was found corrosion leakage of a large number of 304L stainless steel tubes during the water leakage test. Through field investigation, sampling, chemical composition and mechanical properties test, metallographic analysis, corrosion area surface morphology and micro area component analysis, corrosion reasons were analyzed. The main reason for corrosion is improper installation. Stainless steel tubes were polluted by rain, soil, welding slag during the installation process. Carbon steel members cut the tubes when wore tubes, and was placed in such condition for a too long time. Moreover, the electric current occurred in repair welding with water may accelerate pitting holes.
机译:在使用之前,在漏水测试期间发现了600 MW单元的新冷凝器的腐蚀泄漏了大量的304L不锈钢管。通过现场调查,取样,化学成分和机械性能试验,分析了金相分析,腐蚀面积形态和微区域成分分析,腐蚀原因进行了分析。腐蚀的主要原因是安装不当。不锈钢管被雨,土壤,焊渣在安装过程中污染。碳钢构件在磨损管时切割管,并在此类条件下置于较长的时间。此外,用水修复焊接中发生电流可以加速点孔。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号