In this research, the polyurethane adhesive based on modified rubber seed oil with toluene diisocyanates was successfully synthesized in presence of DBTL catalyst. The chemical structure of modified rubber seed oil was characterized by ~1H-NMR. The suitable reaction time of the polyurethane adhesive synthesis was 4h by providing with FT-IR technique. The effects of NCO index and chain extender (1,4-butane diols) content in adhesive formulation as well as cure temperature were also studied by leather to leather on adhesion peel strength. It was found that the higher NCO index or chain extender content gave the higher adhesion of substrate. The cure temperature of adhesive at 70°C gave the better peel strength than that at 30°C during 24 h.
机译:在该研究中,在DBTL催化剂存在下成功地合成了基于改性橡胶籽油的聚氨酯粘合剂。改性橡胶种子油的化学结构的特征在于〜1H-NMR。通过提供FT-IR技术,聚氨酯粘合剂合成的合适反应时间为4H。通过皮革对粘合剥离强度的皮革,还研究了NCO指数和链烷增长(1,4-丁烷二醇)含量以及固化温度的影响。发现较高的NCO指数或链增量含量含有较高的基材粘附性。在70℃下,粘合剂的固化温度在24小时期间,在30℃下呈现更好的剥离强度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号