首页> 外文会议>International Conference on Renewable Energy and Environmental Technology >Characterization, Dissolution and Solubility of Pyromorphite Pb_5(PO_4)_3Cl at 25°C
【24h】

Characterization, Dissolution and Solubility of Pyromorphite Pb_5(PO_4)_3Cl at 25°C

机译:致丙酸酯PB_5(PO_5(PO_5)在25°C时的表征,溶解和溶解性

获取原文
获取外文期刊封面目录资料

摘要

Pyromorphite was synthesized by precipitation and characterized by various techniques. The batch dissolution experiment was conducted at 25°C and different initial pHs (2, 4 and 6). The solid phase showed no obvious change before and after dissolution. The aqueous phosphate concentration decreased quickly from 0.22 to 0.01 mmol/L and then increased very slowly with time. After 2160 h dissolution, it reached a steady-state value of about 0.13 mmol/L. The aqueous lead concentration increased initially and reached a peak value after 72 h dissolution.
机译:通过沉淀合成吡咯岩,其特征在于各种技术。分批溶解实验在25℃和不同的初始pH(2,4和6)。固相显示出在溶解前和之后没有明显的变化。磷酸水溶液浓度从0.22至0.01mmol / L迅速降低,然后随时间慢慢增加。 2160小时溶解后,它达到稳态值约为0.13mmol /升。含水铅浓度最初增加,并在72小时溶解后达到峰值。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号