Suspension roasting furnace was used as the reactor of magnetic roasting of fine grained siderite, and the N_2 was used as the conveying gas. The results show that, the siderite ore be roasted at the conditions of gas velocity is 1.7m/s, and the roasted time is 12.35s, according to magnetic separation can obtained iron concentrate grade is 65.04%, and recovery rate is 93.03%.
机译:悬浮焙烧炉用作细粒颗粒散热器的磁性焙烧的反应器,并且使用N_2作为输送气体。 结果表明,在气体速度条件下烤盐酸盐矿石为1.7m / s,烘烤时间为12.35s,根据磁性分离,可以获得铁浓缩率为65.04%,回收率为93.03%。