Experimental Study of flotation on high intensity magnetic concentrates of Ilmenite

机译:硅藻土高强度磁性浓缩物的浮选试验研究

获取原文

摘要

In order to improve the separating index of ilmenite to separate the concentrate by high intensity magnetic separation, the Heishan iron ore in Chengde did some work. Separate the sulfide ore out by flotation under the conditions of concentration by weight in feed 32%, consumption of xanthate 200g/t and 2# oil 40g/t. Use sulfate to adjust the pH of the low sulphur product of flotation, the mixture of EM351-2 and EM351-3 as foaming agent, after one roughinging and four fold concentrating, got the final titanium concentrate, the grade of which is 47.23%, and the recovery is 58.29%. During the procedure of roughing, the consumption of the reagent as follows: sulfate 2kg/t, EM351-3 1kg/t, EM351-2 900g/t. The consumption of sulfate during fourfold concentrating is 1kg/t. The index is more stable when the concentration in feed is 18%~26% during flotation. The index is stable during the continuous 26 work time for the process under this reagent system. The screen analysis of the flotation concentrate indicates that this reagent system has a better effect on the flotation of +0.074mm particles, and a bad effect on the flotation of -0.045mm particles.
机译:为了改善Ilmenite的分离指数以通过高强度磁分离将浓缩物分离,成都的Heishan Iron Ore做了一些作品。在饲料32%浓缩条件下用浮选将硫化物矿石分开,黄原酸盐200g / t和2#油40g / t的消耗。用硫酸盐调节浮选的低硫产物的pH,EM351-2和EM351-3的混合物作为发泡剂,一次粗加工和四倍浓缩后,得到最终钛浓缩物,等级为47.23%,回收率为58.29%。在粗加工过程中,试剂的消耗如下:硫酸盐2kg / t,em351-3 1kg / t,em351-2 900g / t。四重浓度硫酸盐的消耗是1kg / t。当浮选期间饲料中的浓度为18%〜26%时,指数更稳定。该指数在该试剂系统下的过程中连续的26工作时间稳定。浮选浓缩物的筛网分析表明,该试剂系统对+ 0.074mm颗粒的浮选具有更好的影响,以及对-0.045mm颗粒的浮选的不良影响。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号