首页> 外文会议>International Workshop on Functional Materials >Structure and Magnetic Properties of Co-doped ZnO Dilute Magnetic Semiconductors Synthesized via Hydrothermal Method
【24h】

Structure and Magnetic Properties of Co-doped ZnO Dilute Magnetic Semiconductors Synthesized via Hydrothermal Method

机译:通过水热法合成的共掺杂ZnO稀磁半导体的结构和磁性性能

获取原文

摘要

Using X-Ray Diffraction, Scanning Electron Microscopy, and Superconducting Quantum Interference Device magnetometer, detailed structural, morphological, and magnetic properties are reported on undoped and cobalt doped ZnO Dilute Magnetic Semiconductors, which were prepared by the hydrothermal method. Synthesis of undoped ZnO and cobalt-doped ZnO nanorods was carried out using aqueous solutions of Zn(NO_3)_2.6H_2O, Co(C_2H_3OO)_2.4H_2O, and NH_4OH as hydrolytic catalyst. Samples of different sizes and shapes were synthesized by varying process parameters such as solution molarity (0.05M, 0.15M, 0.3M, 0.5M), pH of the precursors in the range 8-11, growth temperature (100°-130°C), growth time (3-6 hrs), and annealing time. Optimum synthesis parameters to grow ZnO and cobalt-doped ZnO nanorods have been obtained. These nanorods show paramagnetic-like behavior. Our results do not indicate ferromagnetism behavior, unlike reported in thin films and nanocrystalline samples. The differences are likely due to the possible role of nanoparticle size, shape, and different oxygen vacancy concentrations.
机译:使用X射线衍射,扫描电子显微镜和超导量子干涉装置磁力计,在未掺杂的和钴掺杂的ZnO稀释磁半导体上报道了详细的结构,形态和磁性,由水热法制备。使用Zn(NO_3)_2.6H_2O,CO(C_2H_3OO)_2.4H_2O和NH_4OH作为水解催化剂的水溶液进行未掺杂的ZnO和掺杂掺杂的ZnO纳米棒。通过不同的工艺参数(例如溶液摩尔性(0.05M,0.15M,0.3M,0.5M),在8-11的前体,生长温度(100°-130℃)的pH值(100°-130℃)的pH,合成不同尺寸和形状的样品。 ),生长时间(3-6小时)和退火时间。已经获得了生长ZnO和掺杂钴ZnO纳米棒的最佳合成参数。这些纳米棒显示出柔顺的行为。我们的结果不表示铁磁性行为,与薄膜和纳米晶样品不同。差异可能是由于纳米粒子尺寸,形状和不同氧空位浓度的可能作用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号