Orthogonal test was carried out to investigate effects of multiple factors during the magnetization roasting-magnetic separation process as follow: roasting temperature, time, ratio of reducing agent and magnetic field intensity. Significant order of those factors on grade of iron concentrate is obtained, and opportune condition for magnetic roasting is determined. As the condition that roasting temperature is 850°C, time is 40min, ratio of reducing agent is m_(coal)/m_(ore)=12% and magnetic field intensity is 1800Gs, iron ore concentrate whose grade and recovery are 56.32% and 94.03%, respectively, is obtained. At last, through closed-circuit test including magnetization roasting, magnetic separation and reverse flotation, final result is obtained that iron concentrate with phosphorus and silicon are 0.18% and 2.63%, respectively, and its iron grade and recovery are 60.47% and 80.1%, respectively.
机译:进行正交试验,以研究磁化焙烧 - 磁分离过程中多因素的效果如下:焙烧温度,时间,还原剂和磁场强度的比例。获得了铁浓缩物级等因素的重要顺序,确定了磁性焙烧的适当条件。作为焙烧温度为850℃的条件,时间为40分钟,还原剂的比例为M_(煤)/ m_(矿石)= 12%,磁场强度为1800gs,铁矿石浓缩剂的等级和回收率为56.32%分别获得94.03%。最后,通过包括磁化焙烧,磁性分离和反向浮选的闭环试验,获得最终结果,其中具有磷和硅的铁浓缩物分别为0.18%和2.63%,其铁级和回收率为60.47%和80.1% , 分别。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号