Tensile test at ambient temperature, tensile test at high temperature and high temperature tensile creep test were carried out before remnant life prediction. According to the high temperature tensile creep test data, the relationship between working stress, working temperature and rupture life was obtained by MATLAB surface fitting tool. In order to obtain the temperature field and stress field of the superheater tube, ANSYS software was used. Then, the remnant life of the superheater tube was predicted by the extrapolating method and the relationship between working stress, working temperature and rupture life.
机译:在环境温度下拉伸试验,在残余寿命预测之前进行高温和高温拉伸蠕变试验的拉伸试验。根据高温拉伸蠕变试验数据,Matlab表面配件工具获得了工作应力,工作温度和破裂寿命之间的关系。为了获得过热器管的温度场和应力场,使用ANSYS软件。然后,通过外推方法和工作应力,工作温度和破裂寿命之间的关系预测过热器管的残余寿命。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号