Study on the Workability of Self-Compacting Lightweight Aggregate Concrete with Orthogonal Experiment Method

机译:具有正交实验方法自压式轻质骨料混凝土的可加工性研究

获取原文

摘要

In order to get the workability requirements of the preparation of self-compacting lightweight aggregate concrete, fixed sand and gravel volume method and overall calculation method are used in this article to calculate the mix of SCLC30. Orthogonal table L_9 (3~4) is used for test design. In order to analysis the factors of gravel dosage coefficient, sand dosage coefficient, fly ash replace ratio and superplasticizer usage has great influence on concrete by slump flow, L-box and steel-ring tests. The result shows that the groups of 1,3,7,8 have the best workability in 9 groups. On the basis of analysis, gravel coefficient of 0.5, sand coefficient of 0.42, fly ash of 30% and superplasticizer of 1.5% are selected for the optimal mix, so this group has an excellent workability.
机译:为了获得制备自压式轻质骨料混凝土的制备的可加工性要求,本文使用固定砂和砾石体积法和整体计算方法来计算SCLC30的混合。正交表L_9(3〜4)用于测试设计。为了分析砾石剂量系数的因素,砂剂系系,粉煤灰替代比和超增塑料使用对混凝土的坍落度,L箱和钢环试验有很大影响。结果表明,1,3,7,8的组具有9组的最佳可加工性。在分析的基础上,砾石系数为0.5,砂系数为0.42,粉煤灰为30%,过度塑化剂为1.5%的最佳混合,因此该组具有出色的可加工性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号