Experimental Investigation on Flexural Behavior of 500 MPa Reinforced Concrete Beams with and without skin reinforcement

机译:500MPa钢筋混凝土梁加筋与不加筋受弯性能试验研究

获取原文

摘要

Fourteen concrete beams reinforced with 500 MPa longitudinal steel bars, of which 6 with skin reinforcement and 8 without skin reinforcement, were tested under two-point symmetrical concentrated static loading to investigate their flexural behavior. The results indicate that the flexural behavior and deflection mode of test beams with skin reinforcement are basically consistent with those of test beams without skin reinforcement. The use of skin reinforcement can significantly reduce average crack spacing and short-time maximum crack width. And the use of skin reinforcement can also slightly increase the short-time stiffness. Under the serviceability limit state, mid-span deflections are in good agreement with the calculated values according to formula in GB50010-2010. However most of calculated average crack spacing and short-time maximum crack width are larger than measured values. According to the test results, the normal formula of crack width should be revised.
机译:对14根采用500MPa纵向钢筋加固的混凝土梁进行了两点对称集中静载试验研究,其中6根采用蒙皮钢筋,8根不采用蒙皮钢筋。结果表明,有蒙皮加固的试验梁与无蒙皮加固的试验梁的受弯性能和挠度模式基本一致。使用蒙皮钢筋可以显著减少平均裂缝间距和短时最大裂缝宽度。而蒙皮加固的使用也可以略微增加短时刚度。正常使用极限状态下,跨中挠度与GB50010-2010公式计算值吻合较好。然而,大多数计算的平均裂纹间距和短时最大裂纹宽度都大于实测值。根据试验结果,应修正裂缝宽度的常规公式。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号