首页> 外文会议>International conference on advanced materials >Preparation of Low-heat Portland Cement Clinker with Coal Gangue
【24h】

Preparation of Low-heat Portland Cement Clinker with Coal Gangue

机译:用煤矸石的低温波特兰水泥熟料制备

获取原文

摘要

A kind of low-heat Portland cement clinker was prepared with coal gangue, limestone and gypsum through optimizing the mix proportion of raw materials, and its properties and hydration characteristics were studied. The results showed that the cement clinker meeting the demands of mid (low)-heat Portland cement standard could be prepared with 35% (by weight, the same below) coal gangue, 57-60% limestone and 6-8% gypsum. The raw materials were burned at 1380°C for 40 minutes. The main hydrates were calcium silicate hydrate (C-S-H) gel, ettringite (AFt), monosulfate (AFm) and Ca(OH)_2.
机译:通过优化原材料的混合比例,用煤矸石,石灰石和石膏制备一种低热量的波特兰水泥熟料,研究了其性质和水化特性。结果表明,水泥熟料满足MID(低) - 热门水泥标准的需求,可以用35%(重量,以下)煤矸石,57-60%石灰石和6-8%石膏。将原料在1380℃下燃烧40分钟。主要水合物是硅酸钙水合物(C-S-H)凝胶,Ettringite(AFT),单硫酸盐(AFM)和Ca(OH)_2。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号