The 4.5mm wide 25μm thick Fe_(78)Si_9B_(13) amorphous alloys were prepared by single-roller method, and it was annealed. The elastic modulus, tensile deformation and line expansion coefficient were investigated by Q800 (dynamic mechanical thermal analyses, DMA). The results showed that the elastic modulus, tensile deformation and line expansion coefficient were enhanced when annealed. Comparing with the annealed ribbons, the change rules of elastic modulus, tensile deformation and line expansion coefficient of the quenched are evident, that the elastic modulus decreases and tensile deformation increase with temperature increases, but line expansion coefficient firstly increase then decrease with temperature increases.
机译:通过单辊方法制备4.5mm宽的25μm厚Fe_(78)Si_9b_(13)无定形合金,退火。 Q800研究了弹性模量,拉伸变形和线膨胀系数(动态机械热分析,DMA)。结果表明,在退火时增强了弹性模量,拉伸变形和线膨胀系数。与退火的丝带相比,淬火的弹性模量,拉伸变形和线膨胀系数的变化规则是明显的,即弹性模量减小和张力变形随温度升高而增加,但线膨胀系数首先增加随温度的增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号