Separate the Anshan-type Low-grade Hematite Ore With Process of Low-High Intensity Magnetic Separation and Reverse Flotation Method

机译:用低强度磁分离和反向浮选方法的工艺分离鞍山型低级赤铁矿矿石

获取原文

摘要

According to the nature of the ore which containing hematite and magnetite, under the conditions, for example, ore grade is 24.07%, the first fineness of grinding -200 mesh is 50%, the second fineness of grinding -200 mesh is more than 93%, it is concluded that concentrating circuit consisting of first grind-Feebleness magnetic separation -high intensity magnetic separation, second grind-second-high intensity magnetic separation- reverse flotation. Ultimately, A concentrate with a productivity of 18.90%, a grade of 65.21% TFe and the recovery of 51.29% was yielded.
机译:根据含有赤铁矿和磁铁矿的矿石的性质,在例如矿石等级为24.07%,研磨-200目的第一细度为50%,研磨-200目的二次细度大于93 %,得出结论,集中电路由第一研磨 - 虚度磁分离 - 高强度磁分离,第二磨削第二高强度磁分离浮选。 最终,生产率为18.90%的浓缩物,等级为65.21%TFE,恢复为51.29%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号