Study on the Sorption of Rhenium by Anion Exchange Resin

机译:阴离子交换树脂的铼吸附研究

获取原文

摘要

Techniques are applied for the sorption of rhenium from the leaching solution of the fume of calcinating molybdenite concentrate by 201×7 strong base anion exchange resin. By analyzing the main ion from the leaching solution be pretreatmented, the 201×7 strong base anion exchange resin be used in experiment. The influencing factors on the sorption were investigated, with medium pH, the existing form of the ion in the solution and the pH are greatly related to the ion exchange capacity, the result show that the resin not only have higher adsorption rate of (ReO_4)~-, but also have higher separation factor of (ReO_4)~- and (MoO_4)~(2-) when the leaching solution was pretreated pH at 9.0. The separation factor of (ReO_4)~- and (MoO_4)~(2-) reached to 980.5. 5%NH_4OH+9%NH_4Cl solution is a effective desorption reagent for molybdenum, the desorption rate is 96% and nitric acid solution is a effective desorption reagent for rhenium on the loaded resin after desorpted the (MoO_4)~(2-),the desorption rate of (ReO_4)~- is 98%.
机译:通过201×7强基团A阴离子交换树脂将钙钼酸盐浓缩液的浸出溶液应用于铼的技术。通过从浸出溶液中分析主要离子预处理,201×7强基团阴离子交换树脂用于实验。研究了对吸附的影响因素,中期pH,溶液中的离子的现有形式与离子交换能力大大相关,结果表明,树脂不仅具有较高的吸附速率(REO_4) 〜 - ,但也具有更高的分离因子(REO_4)〜 - (MOO_4)〜(2-),当浸出溶液在9.0时pH预处理pH。 (REO_4)〜 - (moo_4)〜(2-)的分离因子达到980.5。 5%NH_4OH + 9%NH_4Cl溶液是用于钼的有效解吸试剂,解吸速率为96%,硝酸溶液是在未解离(Moo_4)〜(2 - )之后加载树脂上的铼对铼的有效解吸试剂。 (REO_4)〜 - 的解吸速率为98%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号