The dump temperature and mixing interval between rubber, silica and silane coupling agent for silica-filled natural rubber (NR) tire tread compounds using bis-triethoxysilylpropyl tetrasulfide (TESPT) as silane were optimized. The dump temperature turns out to be the key parameter governing the properties of the silica-filled NR compounds. The increase in viscosity of the compounds by changing the dump temperature from 100-150°C indicates that inevitably some cross- linking of NR occurs by sulfur contained in TESPT, simultaneous with the silanization reaction between silica and silane. However, the viscosity decreases again when dump temperatures above 150°C are applied, indicating a dominant occurrence of degradation of the NR-molecules. The results are in good agreement with bound rubber contents. The overall properties indicate that a dump temperature in the range of 135-150°C and a silica-silane-rabber mixing interval of 10 minutes are the most appropriate mixing conditions for silica-filled NR compounds with TESPT as coupling agent. Keywords: silica; natural rubber; silane; reinforcement; mixing
机译:使用双 - 三乙氧基甲硅烷四硫化物(TESPT)作为硅烷二氧化硅填充的天然橡胶(NR)轮胎胎面配料转储温度和橡胶,二氧化硅和硅烷偶联剂之间的混合的时间间隔进行了优化。转储温度原来是管辖二氧化硅填充的NR化合物的性质的关键参数。通过改变从100-150转储温度中的化合物的粘度的增加℃下表示NR的不免有些交联由包含在TESPT硫,同时用二氧化硅和硅烷之间的反应的硅烷化发生。然而,粘度再次降低时转储温度在150℃以上被施加,表示NR-分子的降解的显性发生。该结果与结合橡胶的内容一致。总体性质表明,在135-150℃的范围内和10分钟的二氧化硅的硅烷rabber混合间隔转储温度对于二氧化硅填充的NR化合物与TESPT作为偶联剂的最适当的混合条件。关键词:二氧化硅;天然橡胶;硅烷;加强;混合

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号