The layered, machinable ternary compound, T13AIC2, was corrosion-tested at 800, 900, and 1000°C under an Ar-1% SO2 gas atmosphere,. The scale formed consisted primarily of T1O2 and (X-AI2O3, As the corrosion progressed, the scale became thicker and developed into an outer TiC>2 layer and an inner (TiC>2,Al2O3)-mixed layer.
机译:层状的可加工三元化合物T13Aic2在Ar-1%SO2气氛下在800,900和1000℃下腐蚀测试。形成的刻度主要由T1O2和(X-Ai2O3,随着腐蚀所进播的,所述刻度变厚,并发展到外部Tic> 2层和内(Tic> 2,Al2O3) - 夹层层。