INCREASING ANODE THICKNESS TO OPTIMISE COPPER PRODUCTION AT THE KIDD METALLURGICAL SITE

机译:增加阳极厚度,以优化KIDD冶金部位的铜生产

获取原文

摘要

In recent years, improved operation of the Kidd smelter has resulted in an increase in blister production capacity. Due to manpower and equipment limitations anode production and treatment rates could not be increased without incurring significant additional operating expenses. The option chosen to expand casting and refinery capacity to meet the available blister supply was to increase the anode thickness while maintaining the same anode exchange cycle in the refinery. This has resulted in a cathode production increase of almost 10 percent for minimal expenditure. Equipment and process modifications required to cast and refine the thicker anodes are discussed in this paper, along with the Six Sigma methodologies used to identify them. Key areas covered are Hazelett continuous caster operation, refining process parameters, plating performance and cathode quality.
机译:近年来,基德冶炼厂的改进运作导致水泡生产能力增加。由于人力和设备限制,阳极生产和治疗率不会增加,而不会产生大量额外的营业费用。选择扩展铸造和炼油厂以满足可用泡罩供应的选项是增加阳极厚度,同时保持炼油厂中相同的阳极交换循环。这导致阴极产量增加近10%,以实现最低支出。本文讨论了铸造和精炼较厚阳极所需的设备和工艺修改,以及用于识别它们的六种Sigma方法。覆盖的关键区域是Hazelett连续脚轮操作,精炼工艺参数,电镀性能和阴极质量。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号