首页> 外文会议>Paint and Coating Exposition >AN OUNCE OF PREVENTION… THE RELIABILITY OF FIELD METHODS FOR DETECTING THE PRESENCE OF AMINE BLUSH ON EPOXY COATINGS
【24h】

AN OUNCE OF PREVENTION… THE RELIABILITY OF FIELD METHODS FOR DETECTING THE PRESENCE OF AMINE BLUSH ON EPOXY COATINGS

机译:一盎司预防......检测胺腮红存在于环氧涂料上的现场方法的可靠性

获取原文

摘要

Shop and field conditions of high humidity and cool temperature during curing of amine-cured epoxy coatings can produce a haze or oily residue on the surface. This is commonly referred to as "amine blush." The residue is caused by the presence of unreacted amine on the surface of the epoxy coating reacting with carbon dioxide and moisture in the air to form a carbamate. The reaction is propagated by cool temperatures, and is exacerbated by increased film thickness and excess carbon dioxide (e.g., via use of portable gas heaters). If undetected, the presence of an amine blush (in sufficient quantities) can cause intercoat delamination once the "blushed" coating is recoated.
机译:在固化胺固化的环氧涂层期间的高湿度和凉爽温度的商店和现场条件可在表面上产生雾度或油性残留物。这通常被称为“胺腮红”。残留物是由在环氧涂层表面上的未反应胺存在与空气中的二氧化碳反应的未反应胺存在引起的,以形成氨基甲酸酯。反应通过冷温度繁殖,通过增加的膜厚度和过量的二氧化碳加剧(例如,通过使用便携式气体加热器而加剧。如果未检测到,一旦重新涂覆“腮红”涂层,胺腮红的存在(足够量)会导致底涂层分层。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号