Fine polyimide beads were obtained by thermal dehydration reaction of fine poly(amic acid) beads, which were prepared by mixing tetracarboxylic acid dianhydride solution with diamine solution using micro-flow-mixing devices. The diameter of these beads, which could be controlled from submicron to several microns, had a coefficient of variation less than 10%.