Properties of alumina slurry prepared by wet jet milling were investigated. The viscosity and panicle size distribution were measured. Wet jet milled slurry had very lower viscosity than ball milled slurry. The viscosity of wet jet milled slurry was about 6mPa centre dot s and invariable for a long time. On the other hand, the viscosity of ball milled slurry increased rapidly with time and reached a maximum. The particle size distribution of wet jet milled slurry corresponded with the ball milled slurry.